Abstract
This test method covers the determination of bitumen content in materials containing at least 25 % bitumen. The sample shall be representative, and if it contains more than 2 % of water it shall be dehydrated. The procedures for the determination of bitumen content in materials are presented in details.
This abstract is a brief summary of the referenced standard. It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application. ASTM does not give any warranty express or implied or make any representation that the contents of this abstract are accurate, complete or up to date.
1. Scope
1.1 This test method covers the determination of bitumen content in materials containing at least 25 % bitumen. Bitumen content may usually be expeditiously and accurately determined by Procedure No. 1, Section 7. However, some bituminous materials containing finely divided mineral matter may clog the filter or the mineral residue may not be easily retained, in which cases Procedure No. 2, Section 8, shall be followed.
1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability and regulatory limitations prior to use. For specific precautionary information, see Section 4.
2. Referenced Documents
D370 Test Method for Dehydration of Oil-Type Preservatives
E177 Practice for Use of the Terms Precision and Bias in ASTM Test Methods
Index Terms
bitumen; coal tar; solubility; ICS Number Code 91.100.50