Revision of B366/B366M-23 Standard Specification for Factory-Made Wrought Nickel and Nickel Alloy Fittings

Rationale

Add UNS N08935. This grade already appears in other specifications which are cited in this specification as permissible raw materials (B163, B677, B625, B649, B673 (currently being added)). The recommended heat treatment parameters in Table 3 are the some as those found in B649.

Details

Developed by Subcommittee: B02.07

Committee: B02

Staff Manager: Jennifer Tursi

Work Item Status

Date Initiated: 03-24-2025

Technical Contact: Keith Hottle